Seamless Stainless Steel TP446 Pipe
 1.4762 seamless stainless steel pipe

Seamless Stainless Steel TP446 Pipe

Seamless Stainless Steel TP446 Pipe
Seamless Stainless Steel TP446 Pipe stockist and distributor with EN 10204 3.1 certification, custom sizes and export packing.
Request a quote

Send your specification — grade, OD × wall thickness, standard, quantity. Firm quotation within 24 hours; MOQ from 1 piece; EN 10204 3.1 MTC.

TP446 (UNS S44600 / 1.4762) Seamless Stainless Steel Pipe

ASTM A268 · UNS S44600 · EN 1.4762 · Annealed And Pickled · EN 10204 3.1

TP446 is a 25Cr ferritic stainless steel with excellent resistance to oxidation and to sulfur-bearing atmospheres. It avoids the nickel cost of austenitic grades and resists scaling to about 1150 °C in clean oxidizing conditions.

GZH supplies TP446 seamless pipe in 6 – 610 mm OD and SCH 5S – 40 (1 – 25 mm) wall, annealed and pickled, with EN 10204 3.1 certificates as standard and 3.2 on request.

Key specifications

GradeTP446 / UNS S44600 / EN 1.4762 / 10Cr27 (S44600)
Product standardASTM A268 (seamless)
ProcessSeamless — hot extrusion / hot piercing, cold drawn or cold pilgered finishing
Outer diameter6 – 610 mm
Wall thicknessSCH 5S – 40 (1 – 25 mm)
LengthRandom, double random, cut to length up to 18 m
EndsPlain, beveled
Delivery conditionAnnealed and pickled
CertificateEN 10204 3.1 (3.2 on request — ABS, DNV, LR, BV, TÜV)

Chemical composition, % (per ASTM A268)

CMnSiPSCrNiN
≤ 0.20≤ 1.50≤ 1.00≤ 0.040≤ 0.03023.0 – 27.0≤ 0.75≤ 0.25

Mechanical and physical properties

Tensile strength, room temperature≥ 480 MPaASTM A268 minimum
Yield strength (0.2% offset)≥ 275 MPaASTM A268 minimum
Elongation in 2 in. or 50 mm≥ 20%ASTM A268 minimum
Hardness≤ 90 HRB (typical)Published typical value
Density7.6 g/cm³Published typical value
Melting range≈ 1450 – 1500 °CPublished typical value
Thermal expansion, 20 – 100 °C≈ 10.5 µm/m·KPublished typical value
Heat treatment800 – 900 °C, air cooledStandard practice
Standard minimums are those of the product specification; typical values are indicative. The values governing each shipment are those of its EN 10204 3.1 mill test certificate.

TP446 compared with related grades

GradeKey alloyingTypical useWatch out for
TP41012Cr martensiticWear parts, hardwarePoor weldability
TP43017Cr ferriticAppliances, general corrosionNot for welded pressure parts
Comparisons are indicative and apply to the standard product forms; confirm the selection for your exact medium, temperature and design code before specifying.

When to choose TP446, and when not to

Choose TP446 when
  • Sulfur-bearing oxidizing gas attacks nickel-bearing grades.
  • Nickel-free chemistry is required for cost or contamination reasons.
  • Service temperature is high but loads are moderate.
Consider something else when
  • Welding heavy sections: 446 has limited toughness and weldability.
  • Thermal cycling with rapid cooling: 446 is notch-sensitive.
  • Aqueous corrosion service.

Typical applications

Furnace internals
Supports, grates and parts that see sulfur-bearing flue gas.
Heat recuperators
Hot gas recuperator tubes operating above 900 °C.
Kiln furniture
Saggers and trays in oxidizing kilns.

Mill, stock and incoming inspection

  • Every heat comes from our parent mill and arrives with an EN 10204 3.1 certificate stating heat number, chemistry and mechanical results.
  • Mill route, for reference: hot extrusion or hot piercing, then cold drawing or cold pilgering at Xintongda. Stock we hold is finished to these routes.
  • Solution annealed at 1040–1120 °C and water quenched at the mill; pickled or bright annealed to your specification.
  • Mill tests to the standard, plus our own incoming check: PMI/XRF grade verification, dimensions, ovality and surface. Third-party inspection by SGS, BV, TÜV or your nominated agency on request.

Certificates

Every shipment includes an EN 10204 3.1 mill test certificate with heat number, chemistry, mechanical results and test reports. EN 10204 3.2 is available through your nominated inspection agency.

Packing and delivery

Pipes are end-capped, bundled and packed in plywood cases or steel frames for sea freight. Loading port: Shanghai / Ningbo or as requested. Contact us for current lead time and stock sizes.

How to request a quote

Send us: outer diameter, wall thickness or schedule, length, quantity, standard and certificate level, delivery condition, destination port. We reply within 24 hours.
Contact:supply@xtd-ss.com · +86-577-88989817

Frequently asked questions

1. What is TP446 used for?
It is used for furnace internals, heat recuperators, kiln furniture. Supports, grates and parts that see sulfur-bearing flue gas.
2. What is the difference between TP446 and TP410?
TP446 is 27Cr-1Ni; TP410 is 12Cr martensitic. TP410 is typically used for wear parts, hardware, while TP446 is chosen when Sulfur-bearing oxidizing gas attacks nickel-bearing grades. Check the medium, temperature and design code before substituting one for the other.
3. What is the maximum service temperature of TP446?
about 1150 °C in clean oxidizing atmospheres; 980 °C in sulfur-bearing gas. The limit depends on atmosphere, load and cycling; confirm it against the design code and the mill certificate for your heat.
4. Are TP446, UNS S44600 and EN 1.4762 the same material?
Yes. TP446, UNS S44600, EN 1.4762 and 10Cr27 (S44600) are designations of the same grade family in ASTM, UNS, EN and Chinese systems respectively. The certificate states the exact designation supplied.
5. Can TP446 be welded?
Yes, but ferritic grades need limited heat input and careful preheat; use a qualified procedure and avoid heavy sections.
6. What are the main limits of TP446?
Lower toughness and weldability than austenitics, and no benefit in aqueous chloride service.
7. Do you provide mill test certificates?
Yes. EN 10204 3.1 comes with every shipment. EN 10204 3.2 is available with third-party inspection.
8. What are your MOQ and lead time?
MOQ is negotiable by size and quantity. Standard lead time is typically 15 – 30 days depending on the production route; stock sizes can ship faster. Contact us for a firm schedule.
9. Do you manufacture this grade yourself?
No. The pipe is made at our parent mill, Zhejiang Xintongda Special Steel, and we distribute it. That is why the certificate carries a mill heat number and why we can show you the mill’s test records – and also why we can sell you a single length instead of a heat.
Need TP446 seamless pipe for your project?
Send your size list and standard — our engineers reply with a firm offer within 24 hours.