Seamless Copper Nickel 70/30 Pipe
Copper Nickel 70/30 (UNS C71500 / 2.0882) Seamless Copper Nickel Pipe
Copper nickel 70/30 (UNS C71500) has 30% nickel, giving higher strength and better erosion-corrosion resistance than 90/10 in faster seawater and polluted conditions. It is specified for high-velocity condensers and naval piping.
GZH supplies Copper Nickel 70/30 seamless pipe in 6 – 610 mm OD and 0.8 – 12 mm wall, annealed and pickled, with EN 10204 3.1 certificates as standard and 3.2 on request.
Key specifications
| Grade | Copper Nickel 70/30 / UNS C71500 / EN 2.0882 / BFe30-1-1 |
| Product standard | ASTM B466 (seamless); ASTM B552 for tube on request |
| Process | Seamless — hot extrusion / hot piercing, cold drawn or cold pilgered finishing |
| Outer diameter | 6 – 610 mm |
| Wall thickness | 0.8 – 12 mm |
| Length | Random, double random, cut to length up to 18 m |
| Ends | Plain, beveled |
| Delivery condition | Annealed and pickled |
| Certificate | EN 10204 3.1 (3.2 on request — ABS, DNV, LR, BV, TÜV) |
Chemical composition, % (per ASTM B466)
| Cu | Ni | Fe | Mn | Zn | Pb |
|---|---|---|---|---|---|
| balance | 29.0 – 33.0 | 0.40 – 1.00 | ≤ 1.00 | ≤ 1.00 | ≤ 0.05 |
Mechanical and physical properties
| Tensile strength, room temperature | ≥ 370 MPa | ASTM B466 minimum |
| Yield strength (0.2% offset) | ≥ 125 MPa | ASTM B466 minimum |
| Elongation in 2 in. or 50 mm | ≥ 30% | ASTM B466 minimum |
| Hardness | ≈ 70 HRB (typical) | Published typical value |
| Density | 8.94 g/cm³ | Published typical value |
| Melting range | ≈ 1100 – 1145 °C | Published typical value |
| Thermal expansion, 20 – 100 °C | ≈ 16.2 µm/m·K | Published typical value |
| Heat treatment | 600 – 700 °C, water quenched | Standard practice |
Copper Nickel 70/30 compared with related grades
| Grade | Key alloying | Typical use | Watch out for |
|---|---|---|---|
| CuNi 90/10 | 10Ni-Cu-Fe | Seawater piping and condensers | Erosion at high velocity |
| CuNi 70/30 | 30Ni-Cu-Fe | High-velocity seawater | Higher cost |
| Titanium Gr2 | Commercially pure Ti | Seawater condensers | Higher cost |
When to choose Copper Nickel 70/30, and when not to
- Seawater velocity or sand content exceeds 90/10 limits.
- Higher strength and erosion resistance are needed.
- Polluted seawater service.
- Sulfide-bearing water without filtration.
- Weight-critical designs: titanium may be lighter per duty.
- Service above 300 °C.
Typical applications
Mill, stock and incoming inspection
- Every heat comes from our parent mill and arrives with an EN 10204 3.1 certificate stating heat number, chemistry and mechanical results.
- Mill route, for reference: hot extrusion or hot piercing, then cold drawing or cold pilgering at Xintongda. Stock we hold is finished to these routes.
- Solution annealed at 1040–1120 °C and water quenched at the mill; pickled or bright annealed to your specification.
- Mill tests to the standard, plus our own incoming check: PMI/XRF grade verification, dimensions, ovality and surface. Third-party inspection by SGS, BV, TÜV or your nominated agency on request.
Certificates
Every shipment includes an EN 10204 3.1 mill test certificate with heat number, chemistry, mechanical results and test reports. EN 10204 3.2 is available through your nominated inspection agency.
Packing and delivery
Pipes are end-capped, bundled and packed in plywood cases or steel frames for sea freight. Loading port: Shanghai / Ningbo or as requested. Contact us for current lead time and stock sizes.
How to request a quote
Send us: outer diameter, wall thickness or schedule, length, quantity, standard and certificate level, delivery condition, destination port. We reply within 24 hours.