Seamless Incoloy 825 Tube
image
 2.4858 seamless nickel alloy tube

Seamless Incoloy 825 Tube

Seamless Incoloy 825 Tube
Seamless Incoloy 825 Tubes (UNS N08825 / W.Nr. 2.4858) are high-performance nickel-iron-chromium solutions engineered for exceptional resistance to both reducing and oxidizing acids. As the trading and distribution arm of GZH Special Steel (our parent mill), GZH supplies premium seamless tubing stabilized with Titanium to prevent intergranular corrosion after welding.

Our Incoloy 825 seamless pipes comply with ASTM B423 and ASME SB423 standards, offering superior protection against stress-corrosion cracking, pitting, and crevice corrosion in sulfuric and phosphoric acid environments. Through advanced cold-drawing and precise heat treatment,GZH delivers durable, high-strength tubing for chemical processing, marine engineering, and oil & gas applications. Rely on our expertise for certified alloy solutions that meet the most stringent industrial specifications.
Contact Now
add to cart

Incoloy 825 (UNS N08825 / 2.4858) Seamless Nickel Alloy Tube

ASTM B423 · UNS N08825 · EN 2.4858 · Solution Annealed And Pickled · EN 10204 3.1

Incoloy 825 (UNS N08825) is a titanium-stabilised nickel-iron-chromium alloy with molybdenum and copper. It resists sulfuric and phosphoric acids, seawater and oxidizing/reducing acid mixtures, and is a standard material for acid plant and phosphoric acid equipment.

GZH supplies Incoloy 825 seamless tube in 6 – 762 mm OD and SCH 5S – XXS (0.5 – 40 mm) wall, solution annealed and pickled, with EN 10204 3.1 certificates as standard and 3.2 on request.

Key specifications

GradeIncoloy 825 / UNS N08825 / EN 2.4858 / NS1402 / GH825
Product standardASTM B163 (seamless); ASTM B423 for pipe on request
ProcessSeamless — hot extrusion / hot piercing, cold drawn or cold pilgered finishing
Outer diameter6 – 762 mm
Wall thicknessSCH 5S – XXS (0.5 – 40 mm)
LengthRandom, double random, cut to length up to 18 m
EndsPlain, beveled
Delivery conditionSolution annealed and pickled
CertificateEN 10204 3.1 (3.2 on request — ABS, DNV, LR, BV, TÜV)

Chemical composition, % (per ASTM B423)

NiCrMoCuTiFeCMnSi
38.0 – 46.019.5 – 23.52.50 – 3.501.50 – 3.000.60 – 1.20≥ 22.0≤ 0.05≤ 1.00≤ 0.50

Mechanical and physical properties

Tensile strength, room temperature≥ 586 MPaASTM B423 minimum
Yield strength (0.2% offset)≥ 241 MPaASTM B423 minimum
Elongation in 2 in. or 50 mm≥ 30%ASTM B423 minimum
Hardness≤ 100 HRB (typical)Published typical value
Density8.4 g/cm³Published typical value
Melting range≈ 1350 – 1400 °CPublished typical value
Thermal expansion, 20 – 100 °C≈ 13.0 µm/m·KPublished typical value
Heat treatment980 – 1080 °C, water quenchedStandard practice
Standard minimums are those of the product specification; typical values are indicative. The values governing each shipment are those of its EN 10204 3.1 mill test certificate.

Incoloy 825 compared with related grades

GradeKey alloyingTypical useWatch out for
Inconel 60072Ni-15CrHigh-temperature oxidation, causticSulfidation in sulfur gases
Inconel 62558Ni-21Cr-9Mo-NbCorrosion plus high temperatureHigher cost
Hastelloy C276Ni-16Cr-16Mo-WHCl and wet chlorineHigher cost
Comparisons are indicative and apply to the standard product forms; confirm the selection for your exact medium, temperature and design code before specifying.

When to choose Incoloy 825, and when not to

Choose Incoloy 825 when
  • Sulfuric acid service at moderate temperature and concentration.
  • You need resistance to both oxidizing and reducing media.
  • Chloride SCC rules out 904L or 254SMO.
Consider something else when
  • Hydrochloric acid: C276 or B3 are required.
  • Nitric acid above 60% strength.
  • High-temperature creep service above 540 °C.

Typical applications

Sulfuric and phosphoric acid
Heat exchangers, piping and evaporators in acid plant.
Seawater cooling
Tubing resistant to chloride SCC.
Pickling and chemical
Equipment handling mixed acids.

Mill, stock and incoming inspection

  • Every heat comes from our parent mill and arrives with an EN 10204 3.1 certificate stating heat number, chemistry and mechanical results.
  • Mill route, for reference: hot extrusion or hot piercing, then cold drawing or cold pilgering at GZH. Stock we hold is finished to these routes.
  • Solution annealed at 1040–1120 °C and water quenched at the mill; pickled or bright annealed to your specification.
  • Mill tests to the standard, plus our own incoming check: PMI/XRF grade verification, dimensions, ovality and surface. Third-party inspection by SGS, BV, TÜV or your nominated agency on request.

Certificates

Every shipment includes an EN 10204 3.1 mill test certificate with heat number, chemistry, mechanical results and test reports. EN 10204 3.2 is available through your nominated inspection agency.

Packing and delivery

Tubes are end-capped, bundled and packed in plywood cases or steel frames for sea freight. Loading port: Shanghai / Ningbo or as requested. Contact us for current lead time and stock sizes.

How to request a quote

Send us: outer diameter, wall thickness or schedule, length, quantity, standard and certificate level, delivery condition, destination port. We reply within 24 hours.
Contact:supply@xtd-ss.com · +86-577-88989817

Frequently asked questions

1. What is Incoloy 825 used for?
It is used for sulfuric and phosphoric acid, seawater cooling, pickling and chemical. Heat exchangers, piping and evaporators in acid plant.
2. What is the difference between Incoloy 825 and Inconel 600?
Incoloy 825 is 24Cr-46Ni-4Mo; Inconel 600 is 72Ni-15Cr. Inconel 600 is typically used for high-temperature oxidation, caustic, while Incoloy 825 is chosen when Sulfuric acid service at moderate temperature and concentration. Check the medium, temperature and design code before substituting one for the other.
3. What is the maximum service temperature of Incoloy 825?
about 540 °C for pressure service; oxidation resistance to 800 °C. The limit depends on atmosphere, load and cycling; confirm it against the design code and the mill certificate for your heat.
4. Are Incoloy 825, UNS N08825 and EN 2.4858 the same material?
Yes. Incoloy 825, UNS N08825, EN 2.4858 and NS1402 / GH825 are designations of the same grade family in ASTM, UNS, EN and Chinese systems respectively. The certificate states the exact designation supplied.
5. Can Incoloy 825 be welded?
Yes, using matching nickel-alloy filler and clean, low-heat-input procedures; pickling or stainless brushing after welding restores the passive surface.
6. What are the main limits of Incoloy 825?
Limits depend on the alloy: reducing acids, oxidizing salts and sulfur-bearing high-temperature gases each require a specific nickel grade.
7. Do you provide mill test certificates?
Yes. EN 10204 3.1 comes with every shipment. EN 10204 3.2 is available with third-party inspection.
8. What are your MOQ and lead time?
MOQ is negotiable by size and quantity. Standard lead time is typically 15 – 30 days depending on the production route; stock sizes can ship faster. Contact us for a firm schedule.
9. Do you manufacture this grade yourself?
No. The pipe is made at our parent mill, GZH Special Steel, and we distribute it. That is why the certificate carries a mill heat number and why we can show you the mill’s test records – and also why we can sell you a single length instead of a heat.
Need Incoloy 825 seamless tube for your project?
Send your size list and standard — our engineers reply with a firm offer within 24 hours.